Characteristics | Unit | CA slag conditioner |
Chemical analysis(XRF,without LOI) | | Sintered type |
AL2O3 | % | 37-41 |
Fe2O3 | % | ≤2.5 |
SiO3 | % | ≤5.5 |
MgO3 | % | ≤4 |
CaO3 | % | 46-50 |
TiO3 | % | - |
Na2O3 | % | - |
Fe(magnetic) | % | - |
Loss on ignition(1050℃/2h) | % | ≤0.5 |
Moisture(105℃) | % | ≤0.5 |
Characteristics | Unit | CA slag conditioner |
Chemical analysis(XRF,without LOI) | | Sintered type |
AL2O3 | % | 38-42 |
Fe2O3 | % | ≤3 |
SiO3 | % | ≤5 |
MgO | % | 11-15 |
CaO | % | 32-40 |
TiO2 | % | - |
Loss on ignition(1050℃/2h) | % | ≤0.5 |
Moisture(105℃) | % | ≤0.5 |
Specific density of grains | kg/dm3 | |